| Technical properties | Precontraint®1002 T2 back PVDF | Standards |
| Yarn | PES HT 1100 Dtex | TERSUISSE |
| Weight | 1050 g/sqm - 31 oz/sqyd | EN ISO 2286-2 |
| Width | 178 cm | (-1mm/+1mm) |
| Tensile strength (warp/weft) | 420/400 daN/ 5 cm 480/450 Lbs | EN ISO 1421 ASTM D 751-00 Cut Strip Method |
| Tear resistance (warp/weft) | 55/50 daN 105/100 Lbs | DIN 53.363 ASTM D 751-00 Trapezoid Tear Method |
| Adhesion | 12 daN/ 5 cm
| EN ISO 2411 |
| Flame retardancy | M2/NF P92-507 B1/DIN 4102-1 BS 7837 Test 2/NFPA 701 CSFM T19 Class C/ASTM E 108 ASTM E84 VKF 5.2/SN 198898 |
| Surface treatment | Fluotop®T2 (High concentration PVDF) |
| Back side treatment | Weldable PVDF (for a better resistance to pollution of the back side of the fabric) |
| Product application | Static & permanent structures |
| Capitalizes on the excellent PVDF weatheringand without changing the making up process allows a better aesthetical performance of the membrane under any shape and from any angle. The technical data here above are average values with a +/- 5% tolerance. |